1 layer of bubbles, aluminum on one side and white vinyl on the other side |
2 layers of bubbles, aluminum on one side and white vinyl on the other side |
| THICKNESS |
4mm (3/16 in.) |
8mm (3/8 in.) |
| WEIGHT |
291 gr/m2 (0.95 oz/pi2) |
355 gr/m2 (1.16 oz/pi2) |
| ROLL WEIGHT |
13.52 kg (29.74 lbs) |
16.49 kg (36.3 lbs) |
| FLAME SPREAD (white side) |
ASTM E84 Classe 1 or A |
ASTM E84 Classe 1 or A |
| SMOKE DEVELOPMENT (white side) |
ASTM E84 Classe 1 or A |
ASTM E84 Classe 1 or A |
| CRUSHING RESISTANCE |
414 kN/m2 4.22kg/cm2 (60.05 lbs/in2 8647 lbs/pi2) |
414 kN/m2 4.22kg/cm2 (60.05 lbs/in2 8647 lbs/pi2) |
| TENSILE STRENGTH |
3.7 N/mm (21.13 lbs.pi/po.) CAN/CGSB-51.33-M89 |
3.7 N/mm (21.13 lbs.pi/po.) CAN/CGSB-51.33-M89 |
| FLEXIBILITY |
No cracking CAN/CGSB-51.33-M89 |
No cracking CAN/CGSB-51.33-M89 |
| THERMAL RESISTANCE |
RSI 0,70 to RSI 2,57 (R4 to R14.6) depending on the installation |
RSI 0,70 to RSI 2,57 (R4 to R14.6) depending on the installation |
| EMISSIVITY |
0.03 - 0.04 |
0.03 - 0.04 |
| REFLECTIVITY |
0.96 - 0.97 |
0.96 - 0.97 |
WATER VAPOUR PERMEANCE before aging after aging |
CGSB 51.33-M89 ASTM E-96 < 0 ng/ Pa.s.m2 < 1 ng/ Pa.s.m2 |
CGSB 51.33-M89 ASTM E-96 < 0 ng/ Pa.s.m2 < 1 ng/ Pa.s.m2 |
| TEMPERATURE RANGE |
-50C à 93C (-50F à 200F) |
-50C à 93C (-50F à 200F) |
| LINEAR SHRINKAGE |
None |
None |
| THERMAL CONDUCTIVITY (K) at 24C (75F) |
0.0384 (0.27) |
0.0416 (0.293) |
| IMPACT SOUND AND TRANSMISSION LOSS |
ASTM E-492, ASTM C-423, ASTM STP-15C, IIC-52 |
ASTM E-492, ASTM C-423, ASTM STP-15C, IIC-53 |